ЧП Ворон. Электронные компоненты и радиомонтажное оборудование. Микросхемы, транзисторы, реле, резисторы, конденсаторы, паяльное оборудование, припой.
Корзина пуста!
ВХОД ДЛЯ КЛИЕНТОВ

Забыли пароль?
Зарегистрироваться

Шановні клієнти інтернет-магазину!

  У зв'язку зі святкуванням Нового Року ми працюємо за наступним графіком:
• з 31.12.24(Вт) по 02.01.25(Чт) не працюємо
• з 03.01.25(Пт) працюємо в звичайному режимі.

  Інтерет-магазин приймає замовлення цілодобово 24/7 !



Поиск:

Enter a search string or click on the microphone icon and begin speaking.

×
История запросов
ваша история поиска пуста
Whole catalog Materials for production and repairMaterials for the manufacture of printed circuit boardsSoldering mask, liquid tin
Код товара:
031120

Liquid photoresist XR-7000 packing 150 g

Liquid photoresist. UV exposed. Manifestation in alkali, acid-resistant. Packing 150 g (+10).
 Liquid photoresist  XR-7000 packing 150 g
NOT available.
Expected price: 299,80 UAH
from 1 pc : 299,80 UAH
from 3 pcs : 269,90 UAH ( -10,0%)
Prices are indicated at the time of product availability and may change upon receipt

Current balances:

NOT available

Изображение товара

Product description format_size zoom_out zoom_in

Used for the production of printed circuit boards, processing of parts by oxidation, in the process of copper plating, glass matting, nickel plating, etc.

Application:

1.Method.
On the prepared (cleaned, skimmed) board n anosize a thin layer of mask through the stencil, creating protected and exposed areas of the board.
(Similar to silk screen printing).
We expose to the light of an ultraviolet lamp (LEDs, direct sunlight) until solidification.


2. Method.
Apply
a mask in the form of one big drop (the volume is selected experimentally, the excess will flow out)
We cover with mylar film (the second detachable layer from the film photoresist), on top is a photomask, for example, printed on a printer.
Press down on top with glass, align the thickness of the mask, focusing on the color of the mask (the thicker - the darker).
We fix it so that the photomask does not move relative to the board, Expose it with ultraviolet light. We select the time experimentally, it depends on the thickness of the glass, the density of the photomask, the lamp power, the distance from the lamp to the board, temperature, etc.
Open areas will harden, darkened areas will remain in a pasty state, uncured mask is removed using a swab with isopropyl alcohol, nitro solvent, solvent, etc. After removing non-hardened areas, it is recommended to additionally "harden" the board - hold it for some time without protective films, stencils, directly in the rays of ultraviolet light.

Leave your feedback or ask a question

Only this product is discussed here. Off topic comments will be deleted! Please follow the Commenting Rules.

The data presented in the product description are for reference only and may differ from those indicated by the manufacturer.
To carry out technical calculations and obtain the exact parameters of the goods, use the datasheets from the manufacturer's website.

If you need additional information, or you found an error in the description, or have other questions about this product, then our manager will help you: Ярослав unknown

Buy with this product: Посмотреть больше…